In the 2014 edition of the ASME B31.3 Code [1], thick, P-No. 1 carbon steel pipe became exempt from Postweld Heat Treatment (PWHT) under the condition of preheating at 95°C (200℉) and multi-pass welding. The decision whether to apply PWHT or not is left to the designer but no further guideline is provided. The impression is that the need for PWHT is only corrosion/service related, and not beneficial or necessary for the integrity of the piping. Several publications [2][3][4] have addressed these changes and highlighted that this might lead to potentially unsafe situations. This paper will critically review the arguments used for the justification of the PWHT exemption for carbon steel and show that many arguments are invalid or incomplete. It will discuss the implications for the performance of materials and predict possible failure scenarios. It will then provide estimates of typical PWHT cost eliminated by the current rules. It will provide an EPC contractor's perspective on the current ASME B31 rules with practical approaches that may be taken to mitigate the risks. Finally, recommendations to the ASME B31 committees involved in PWHT exemption will be provided.
机译:在2014年版的ASME B31.3代码[1],厚,p-no。 1碳钢管在95°C(200°)和多通焊接的情况下豁免在预热的条件下免于焊接热处理(PWHT)。决定是否申请PWHT或不留给设计师,但没有提供进一步的指导。印象是,对PWHT的需求只是腐蚀/服务有关,而不是管道完整性的腐蚀/服务。几个出版物[2] [3] [4]已经解决了这些变化,并强调这可能导致可能的不安全情况。本文批判地审查了用于碳钢的PWHT豁免的理由的论据,并表明许多参数无效或不完整。它将讨论对材料性能的影响并预测可能的失败情景。然后,它将提供当前规则消除的典型PWHT成本的估计。它将在目前的ASME B31规则上提供EPC承包商的观点,具备可能采取的影响风险。最后,将提供向参与PWHT豁免的ASME B31委员会的建议。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号