During feeding of alumina into a Hall-Heroult cell, rafts floating on the bath surface may be formed. In this study, rafts were created in a laboratory furnace by adding 4 g secondary alumina in industrial bath. Samples were withdrawn from the bath in a time interval between 30 and 300 s. The experiments show that at 970 °C, rafts will be formed within 30 s, and then slowly dissolve again with a constant rate of 0.8 g/min. Pores were found in the samples, giving extra buoyancy to the raft, thus increasing the floating time. Same experimental setup was used to investigate the effect of preheating of alumina, where it was found that coherent rafts will form up to at least 500 °C.
机译:在氧化铝进入大厅 - 灌注器中,可以形成漂浮在浴表面上的筏。在这项研究中,通过在工业浴中加入4g二次氧化铝,在实验室炉中创建筏。在30至300秒的时间间隔中从浴中取出样品。实验表明,在970℃下,将在30秒内形成筏,然后用0.8g / min的恒定速率再次缓慢溶解。在样品中发现孔隙,对筏产生额外的浮力,从而增加了浮动时间。使用相同的实验设置来研究预热氧化铝的效果,发现相干筏将形成高达500℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号