To solve the problem that the sintered liquid phase fluidity characteristic of low silica (w(SiO_2) < 3 wt%) and high silica (w(SiO_2) > 7 wt%)) iron ores were different from actual sintering production with using the common method based on w(CaO)/w(SiO_2), a new improved method based on n(Fe_2O_3)/n(CaO) was proposed. The differences between two methods for iron ore fluidity detection were studied. The results show that when the common method is used to detect the liquid phase fluidity, as the content of SiO_2 increased from 2.12 to 11.68 wt%, the amount of CaO addition augmented from 7.88 to 32.65 wt% and the corresponding fluidity index changed from 0 to 5.68. The fluidity index has a linearly positive correlation with the content of SiO_2. The improved method could significantly reduce the effect of the change of CaO addition on the fluidity characteristic of iron ore which caused by the difference of SiO_2.
机译:为了解决低二氧化硅(W(SiO_2)<3wt%)和高二氧化硅(W(SiO_2)> 7wt%)的烧结液相流动性,铁矿石与使用常见的实际烧结产生不同提出了一种基于W(CAO)/ W(SIO_2)的方法,提出了一种基于N(FE_2O_3)/ N(CAO)的新改进方法。研究了两种铁矿石流动性检测方法之间的差异。结果表明,当使用常用方法检测液相流动性时,随着SiO_2的含量从2.12增加到11.68wt%,CaO添加量从7.88增加到32.65wt%,相应的流动性指数从0变为0到5.68。流动指数与SiO_2的含量具有线性阳性相关性。改进的方法可以显着降低CAO添加对由SiO_2差异引起的铁矿石的流动性特性的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号