At present, the commonly used cement has low tensile strength and low flexural strength, which is a fatal defect of cement materials. It is extremely urgent to conduct research on this shortcoming of cement. In addition, the steel industry steel mill produces a large amount of waste steel slag. The chemical composition of steel slag is similar to that of cement. This experiment makes full use of waste steel slag as raw material to prepare cement to improve the performance of cement materials. Using limestone, sandstone, shale, steel slag and river sand as the main raw materials, through the powder preparation, mixing, calcination, grinding, molding process and performance analysis of raw materials. After the calcination, the cement clinker in the form of a block becomes higher in hardness as the steel slag is incorporated. The higher the calcination temperature, the smaller the steel slag incorporation maximum. When the calcined at 1150 °C is mixed with 17.5% steel slag, a cement with better performance can be obtained.
机译:目前,常用的水泥具有低抗拉强度和低弯曲强度,这是水泥材料的致命缺陷。对水泥缺点进行研究是非常迫切的。此外,钢铁工业钢厂生产大量废钢渣。钢渣的化学成分类似于水泥的化学成分。该实验充分利用废钢渣作为原料,制备水泥以提高水泥材料的性能。采用石灰石,砂岩,页岩,钢渣和河砂作为主要原料,通过粉末制备,混合,煅烧,研磨,模塑过程和原料的性能分析。在煅烧之后,随着钢渣掺入,块形式的水泥熟料变得更高。煅烧温度越高,钢渣掺入越大。当1150°C的煅烧与17.5%钢渣混合时,可以获得具有更好性能的水泥。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号