Polymer materials used in domestic hot water heating systems must maintain mechanical properties in the working fluid over their target lifetimes. In potable water, chlorine and pH combine to create an oxidative environment, characterized by the oxidative reduction potential (ORP) that can chemically attack a polymer, resulting in permanent loss of mechanical strength and increase in creep compliance. Polymer morphology data and mechanical property data are presented for polysulfone (PSU), polybutylene (PB), polypropylene random copolymer (PP-r) and polyamide 6/6 (PA66) specimens that had been exposed to an aqueous oxidative environment. The data obtained after up to 1500 hours exposure in hot potable chlorinated water (ORP ranging from 550 mV to 825 mV), show that PSU and the polyolefins with antioxidant additives (PB and PP-r) maintain their mechanical properties, while PA66 degrades significantly.
机译:家用热水加热系统中使用的聚合物材料必须在其目标寿命内保持工作流体的机械性能。在饮用水中,氯和pH会结合在一起形成氧化环境,其氧化还原电位(ORP)可以化学侵蚀聚合物,导致机械强度的永久损失和蠕变柔韧性的提高。提供了已暴露于水氧化环境的聚砜(PSU),聚丁烯(PB),聚丙烯无规共聚物(PP-r)和聚酰胺6/6(PA66)样品的聚合物形态数据和力学性能数据。暴露于热食氯化水中(ORP范围从550 mV至825 mV)长达1500小时后获得的数据表明,PSU和具有抗氧化剂的聚烯烃(PB和PP-r)保持了其机械性能,而PA66则显着降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号