It is nearly twenty years since warm compaction processing (ANCORDESNE) was introduced commercially, permitting medium to large size ferrous PM parts to be compacted to a green density of 7.3 g/cm~3 via single-compaction processing. Subsequent application of the technology will be reviewed along with more recent refinements of the process.