EFFECT OF ORDINARY MAGNETITE RATIOS ON PROPERTIES, PRODUCTIVITY, AND STRENGTH OF HONGGE HIGH-CHROMIUM VANADIUM-TITANIUM MAGNETITE SINTERS

机译:普通磁铁矿对Hipge High-Chermium钒 - 钛磁铁矿山脉性能,生产率和强度的影响

获取原文

摘要

The sintering pot test was used to research the influence of ordinary magnetite (OM) ratios on Hongge high-chromium vanadium-titanium magnetite (HCVTM) sinters. The yield, sintering ratio, tumbler index (TI), productivity, solid fuel consumption, reduction degradation index (RDI) and reduction index (RI) were tested and calculated. In this work, the yield decreases from 90.5% to 84.6%, and sinter ratio decreases slightly from 84.98%) to 83.43%) with increasing OM ratios. The maximum of productivity is 3.52 t-m~(-2)-h~(-1) with 15% OM. The TI first decreases and then increases with increasing OM ratios, and the minimum of TI is 43.65% with 45% OM. The RI increases from 50.7% to 70.9%, and the solid fuel consumption rises from 55.25 kg-t"1 to 59.10 kg-t"1 while the RDI deteriorates from 96.7% to 50.7%) with increasing OM ratios.
机译:烧结罐试验用于研究普通磁铁矿(OM)比对Hupge高铬钒 - 钛磁铁矿(HCVTM)烧结的影响。测试并计算测试和计算产率,烧结比,倒闭器指数(Ti),生产率,固体燃料消耗,还原降解指数(RDI)和还原指数(RI)。在这项工作中,产量从90.5%降至84.6%,并且烧结比略微降低84.98%)至83.43%,随着OM比率增加。生产率的最大值为3.52 T-M〜(-2)-H〜(-1),15%OM。 Ti首先降低,然后随着常规比率的增加而增加,并且Ti的最小值是43.65%,45%OM。 RI从50.7%增加至70.9%,固体燃料消耗从55.25kg-t“1至59.10kg-t”1上升,而RDI从96.7%升高到50.7%),随着常规比率增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号