Deoiled asphalt and titanium were milled by a planet ball milling in order to prepare TiC and examine the cracking behaviors of deoiled alphalt. The milled powder samples were characterized by X-ray diffraction (XRD) measurement and scanning electron microscope (SEM). The produced gases were analyzed by gas phase chromatography. The results indicated that the C-C bonds of the aromatic rings were broken into actived carbon atoms during milling process because of the inductive effect of Ti atoms. The carbon atoms provided element C for the fabrication of TiC by mechanical alloying. The H atoms of aromatic rings were released to form H<,2> The side chains are cracked into CH<,4> and C<,2>H<,6>. The effects of C/Ti ratio and the milling time on mechanical cracking and alloying were discussed in detail.
机译:由行星球磨机研磨的含量沥青和钛以制备TIC并检查糊化的抗碎屑的开裂行为。通过X射线衍射(XRD)测量和扫描电子显微镜(SEM)以研磨的粉末样品为特征。通过气相色谱法分析产生的气体。结果表明,由于Ti原子的诱导效果,在研磨过程中将芳环的C-C键分解成活性炭原子。碳原子通过机械合金化提供了用于制造TIC的元素C.释放芳环的H原子以形成H 2,2>侧链裂化成CH <,4>和C <,2> H 6>。详细讨论了C / Ti比和研磨时间对机械开裂和合金化的影响。

著录项

  • 来源
  • 会议地点
  • 作者

  • 作者单位
  • 会议组织
  • 原文格式 PDF
  • 正文语种
  • 中图分类 TE626.25;
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号