THE MICROSTRUCTURE AND DIELECTRIC PROPERTIES OF Sm_2O_3 DOPED Ba_(0.6)Sr_(0.4)TiO_3-MgO COMPOUND FOR PHASE SHIFTERS

机译:SM_2O_3掺杂BA_(0.6)SR_(0.4)TiO_3-MGO化合物的微结构和介电性能进行相移换体

获取原文

摘要

The structural, surface morphological, tunable and dielectric properties of Sm_2O_3 doped Ba_(0.6)Sr_(0.4)TiO_3-MgO ceramics were investigated. Sm_2O_3 dopant effectively decreases the dielectric loss of BST-MgO ceramics. 0.2wt% Sm_2O_3 additives dramatically weaken the uniform of grains distribution and deteriorated the tunable ability. More uniform grains were observed with higher Sm_2O_3 concentration. The ε-E~2 characteristic is an indicator of the uniformity of grains in BST-MgO composite. For 1.2wt% Sm_2O_3 doped samples, the microwave loss at 2.5GHz is 0.00478 and the tunability is 6.52%, it basically meets the requirements of phase shifters.
机译:研究了SM_2O_3掺杂BA_(0.6)SR_(0.4)TiO_3-MgO陶瓷的结构,表面形态,可调谐和介电性能。 SM_2O_3掺杂剂有效地降低了BST-MgO陶瓷的介电损耗。 0.2wt%sm_2O_3添加剂显着削弱了晶粒分布的均匀,并劣化了可调谐能力。以较高的SM_2O_3浓度观察更均匀的晶粒。 ε-e〜2特征是BST-MgO复合材料中晶粒均匀性的指标。对于1.2wt%SM_2O_3掺杂样品,2.5GHz的微波损耗为0.00478,可调性为6.52%,它基本满足相移器的要求。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号