The new experimental method was developed by use of L-shaped test pieces. The corroded L-shaped test piece was cut and polished to measure the residual size. In order to evaluate the corrosion resistance against the non-alkaline borosilicate glass, the following samples are chosen, that is, FZ-A (Fused ZrO_2 obtained from skin of ingot), FZ-B (from interior), Zircon and Tin-oxide refractory. FZ-A is slightly corroded though remarkable upward drilling is observed in FZ-B and Tin-oxide refractory. It is considered that the differences depend on their microstructure, especially the grain size and homogeneity of the components. The refractory with finer grained homogeneous microstructure shows higher corrosion resistance.
机译:通过使用L形试验片开发了新的实验方法。切割并抛光腐蚀的L形试验片以测量残留尺寸。为了评估对非碱性硼硅酸盐玻璃的耐腐蚀性,选择以下样品,即FZ-A(从锭皮肤获得的熔融ZrO_2),FZ-B(来自内部),锆石和氧化锡耐火。 FZ-A略微腐蚀,但在FZ-B和氧化锡耐火中观察到显着上升钻孔。认为差异取决于它们的微观结构,尤其是组分的晶粒​​尺寸和均匀性。细粒均匀微观结构的耐火性显示出更高的耐腐蚀性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号