首页> 外文会议>International Biohydrometallurgy Symposium >Bioleaching of Complex Refractory Gold Ore Concentrate of China: Comparison of Shake Flask and Continuous Bioreactor
【24h】

Bioleaching of Complex Refractory Gold Ore Concentrate of China: Comparison of Shake Flask and Continuous Bioreactor

机译:中国复杂耐火金矿浓缩物的生物浸渍:摇瓶和连续生物反应器的比较

获取原文

摘要

The laboratory tests of biooxidation and cyanidation were carried out by using samples of the complex refractory gold ore from China. The elemental composition was 16.8% iron, 18.6% sulfur, 4.88% arsenic, 2.30% carbon and 3.49% antimony. Gold is assayed at 46 g/t. The arsenic oxidation of 88.11%, carbon removal rate of 32.34% and antimony oxidation of 23.92% over 16d was achieved in shake flasks in the presence of the mixed culture (HQ0211: Thiobacillus ferrooxidans Leptospirillum ferrooxidans and Thiobacillus thiooxidans). The continuous bioreactor tests resulted in greater dissolution rates for arsenic, carbon and antimony, which led to a greater extent of sulphide oxidation within a shorter period of time. The maximum oxidation of arsenic and antimony was 90.72% and 40.09% respectively and the removal rate of carbon is 63.48% after 8d in the continuous bioreactor tests. After bioleaching, the gold recovery of the oxidation residue was 98.02% with the cyanidation method, which was showed the biological pretreatment was applicable to the complex refractory gold ore.
机译:通过使用来自中国的复杂难熔金矿的样品进行生物氧化和氰化的实验室测试。元素组合物为16.8%铁,18.6%硫,4.88%砷,2.30%碳和3.49%的锑。黄金以46克/吨测定。 (:氧化亚铁硫杆菌钩端螺杆菌和氧化硫硫杆菌HQ0211)的88.11%的砷的氧化,32.34%的碳去除速率和23.92%,比16D锑氧化物在摇瓶中在混合培养物的存在下实现的。连续生物反应器试验造成了更大的溶出速率为砷,碳,锑,这导致硫化物氧化的更短的时间周期内的更大的程度。砷和锑的最大氧化分别为90.72%和40.09%和碳的去除率是在生物反应器中连续测试后8D%63.48。生物浸渍后,氧化残余物的金回收率为98.02%,氰化法显示出生物预处理适用于复合难熔金矿。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号