Up to date, it is difficult to estimate durability of epoxy liner in service time because an estimation of the long term environment-deterioration with aging has not been processed. In the study, the estimation on epoxy liner is carried out by the physical test for 7 rounds. There are the elongation test and the crack bridging test in the part of physical tests. An elongation test is carried out with epoxy membrane and a crack bridging test is carried out with epoxy-coated specimen on mortar. The subjects of test and estimation are a containment quality system and a fibre-glass reinforced system. The materials of these subjects are ET5140, CL890, and EH2340. Ensuring the test data, properties of epoxy liner was estimated and the change of properties was predicted on epoxy liners.
机译:迄今为止,难以在服务时间中估计环氧衬垫的耐久性,因为估计与老化的长期环境 - 恶化仍未得到处理。在研究中,对环氧衬里的估计由7轮物理测试进行。物理测试中有伸长率测试和裂缝桥接试验。用环氧膜进行伸长检测,并在砂浆上用环氧涂层标本进行裂纹桥接试验。测试和估计的受试者是一个容纳质量系统和纤维玻璃增强系统。这些受试者的材料是ET5140,CL890和EH2340。确保测试数据,估计环氧衬垫的性质,并在环氧衬垫上预测了性质的变化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号