The Stress Intensity Factor Dependence of 304 Stainless Steel SCC growth in Deaerated Water

机译:脱气水中304不锈钢SCC生长的应力强度因子依赖性

获取原文

摘要

Stress corrosion crack growth rate (SCCGR) tests wereconducted on 304 stainless steel (SS) in hydrogendeaerated water to characterize the dependence with thestress intensity factor (K). Tests were performed on four304SS heats at 321 and 328°C at K levels that rangedfrom 22 to 89 Mpa√m. Two test strategies were utilizedto quantify the SCCGR K dependence. The majority ofautoclave tests were single or dual specimen tests inwhich multiple K levels were step wise investigated andSCCGRs were evaluated through in-situ direct currentelectrical potential drop. Single K level specimen testswere performed on one 304SS heat at K levels of 25, 51and 74 Mpa√m. Results showed power law SCCGR Kfunctionality with power law exponents which rangedfrom 0.9 to 3.0. The K functionality measured from thesingle condition tests was lower than those measured insingle specimen multiple K conditions tests. The 304SSSCCGR vs. K results, as well as the role of uncrackedligaments on electrical potential drop (EPD) crackgrowth rate measurements and crack openingdisplacement, are discussed.
机译:进行应力腐蚀裂纹扩展率(SCCGR)测试 在氢气中对304不锈钢(SS)进行 用脱气水表征与水的依赖关系 应力强度因子(K)。对四个进行了测试 304SS在321和328°C的K温度范围内加热 从22到89Mpa√m。利用了两种测试策略 量化SCCGR K依赖性。多数的 高压灭菌器测试是单样品测试或双样品测试 逐步检查了多个K水平,以及 SCCGR通过现场直流电进行评估 电势下降。单K级标本测试 在304SS热量下以25、51的K水平进行 和74Mpa√m。结果表明幂定律SCCGR K 幂律指数的功能范围很广 从0.9到3.0。从 单条件测试低于 单个样本,多个K条件测试。 304SS SCCGR vs. K结果,以及完整的作用 韧带上的电位降(EPD)裂纹 增长速率测量和裂缝开度 位移,进行了讨论。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号