Titanium foam is considered as a potential bone substitute because of its good biocompatibility. In the preparation of porous titanium, titanium and cobalt can be distributed evenly in the matrix of porous titanium alloy with cobalt as an alloy element. Such intermetallic compounds possess better mechanical properties. The compressive properties of porous titanium with different cobalt powder addition on it were studied when the volume fraction of urea was 60%, the sintering temperature was 1100 °C, and the holding time was 1.5 h. The results show that with the increase of cobalt content, the compressive properties of porous titanium-cobalt alloy is obviously improved compared with pure porous titanium. When the cobalt content is 10 wt%, the yield strength of the material reaches the maximum value of 363.76 MPa.
机译:钛泡沫由于其良好的生物相容性而被认为是潜在的骨替代物。在制备多孔钛时,钛和钴可以均匀地分布在以钴为合金元素的多孔钛合金基体中。这样的金属间化合物具有更好的机械性能。研究了当尿素的体积分数为60%,烧结温度为1100°C,保温时间为1.5 h时,添加了不同钴粉的多孔钛的压缩性能。结果表明,随着钴含量的增加,多孔钛钴合金的压缩性能明显优于纯多孔钛。当钴含量为10重量%时,材料的屈服强度达到最大值363.76MPa。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号