Effects of pouring temperature and cooling water flux on solidification structure of ferritic stainless steel are investigated with a thermal simulation setup. The results show that with pouring temperatures 1518°C, 1528°C, 1538°C and 1548°C, both L_(mean) (the mean length between columnar to equiaxed transition(CET) position and chill surface of the samples) and the mean dimension of equiaxed grains increase. On the other hand, with cooling water flux 400, 800, 1200 and 1600mL/min, L_(mean) gradually increases, and the mean dimension of equiaxed grains decreases. In addition, low pouring temperature and cooling water flux enlarge the ratio of fine equiaxed grains.
机译:利用热模拟装置研究了浇注温度和冷却水通量对铁素体不锈钢凝固组织的影响。结果表明,在浇注温度1518°C,1528°C,1538°C和1548°C时,L_(均值)(柱状到等轴转变(CET)位置与样品冷表面之间的平均长度)和等轴晶粒的平均尺寸增加。另一方面,当冷却水流量为400、800、1200和1600mL / min时,L_(平均值)逐渐增加,等轴晶粒的平均尺寸减小。另外,低浇注温度和冷却水通量增加了细等轴晶粒的比例。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号