Titanium concentrate and titanium slag were used to prepare high titanium ferroalloy to reduce cost.In the process,the 6-9% of aluminum consumption was replaced by magnesium.The reasonable slag system composition was used.The results indicate that the ferrotitanium of 75% [Ti] and [Al]<4% was prepared.
机译:使用钛浓缩物和钛渣制备高钛铁合金以降低成本。在该过程中,镁用6-9%的铝消耗取代。使用合理的矿渣系统组成。结果表明铁罗托亚硝基制备[Ti]和[Al] <4%。