Modified phenolic resins based on hyperbranched polysiloxane with improved thermal stability and flame retardancy

机译:基于超支化聚硅氧烷的改性酚醛树脂,具有改进的热稳定性和阻燃性

获取原文

摘要

A novel modified phenolic (PF) resin with high performance was developed,which was prepared by hybranched phenyl polysiloxane (HPSi) synthesized by our research group with PF resin.The effect of the incorporation of HPSi into PF resin on typical performance of HPSi/PF resins were systemically discussed.Results show that the incorporation of HPSi can not only effectively promote the thermal properties,but also improve the flame retardancy.For example,in the case of the modified PF resin with 10wt% HPSi,initial decompose temperature (Tdi) of HPSi is at about 405°C,which is 18°C more than that of neat PF resin at the heating rate of 10°C/min; its char yield at 800°C increases from 68.9% to 76.2% at the heating rate of l0°C/min.What's more,HPSi 10/PF resin has the maximum LOI value,which is 14.6% more than that of neat PF resin.The novel modified PF resin with improving integrated properties exhibits great potential to be used for many cutting-edges fields.
机译:课题组以PFSi树脂为研究对象,采用支链聚硅氧烷(HPSi)与PF树脂合成的新型改性酚醛树脂(PFSi),研制了高性能的新型酚醛树脂。PF树脂中掺入HPSi对HPSi / PF典型性能的影响结果表明,掺入HPSi不仅可以有效地提高其热性能,而且可以提高阻燃性。例如,以10wt%的HPSi改性的PF树脂,其初始分解温度(Tdi) HPSi的熔点约为405°C,以10°C / min的升温速率比纯PF树脂高18°C;在10℃/ min的升温速率下,800℃的炭收率从68.9%提高到76.2%。此外,HPSi 10 / PF树脂具有最大的LOI值,比纯PF树脂高14.6%。具有改善的综合性能的新型改性PF树脂具有巨大的潜力,可用于许多前沿领域。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号