The constitutive equation of Ti-6Al-3.5Mo titanium alloy had been researched with thermal simulation experiment. The experimental temperature was between 1030°C and 1120°C, and strain-rate was between 0.001 and 1.0, and the deformation degree was 50 %. According to Arrhenius equation, a kind of constitutive equation of Ti-6Al-3.5Mo titanium alloy had been put forward. Compared the calculation results by constitutive equation with experiment results, the relative errors were less than 12%. For Ti-6Al-3.5Mo titanium alloy, strain-rate sensitivity coefficient being m=0.1688, and temperature sensitivity coefficient being s=10233.
机译:通过热模拟实验研究了Ti-6Al-3.5Mo钛合金的本构方程。实验温度在1030℃至1120℃之间,应变率在0.001至1.0之间,变形度为50%。根据Arrhenius方程,提出了一种Ti-6Al-3.5Mo钛合金的本构方程。将本构方程的计算结果与实验结果进行比较,相对误差小于12%。对于Ti-6Al-3.5Mo钛合金,应变率灵敏度系数为m = 0.1688,温度灵敏度系数为s = 10233。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号