SITUATION OF THE BAFFLE-FORMER BOLTS IN BELGIAN UNITS

机译:比利时单位前挡板螺栓的状况

获取原文

摘要

The baffle to former bolts are used in Pressurized Water Reactors to attach the baffle plates to the former plates in the reactor vessel lower internals. The resulting structure forms a boundary for the flow of coolant and provides lateral support to the fuel assemblies. Some edge bolts are also present, assembling together the baffle plates.After an operating time of the order of 120 000 hours, some bolts exhibit cracking at the junction of the head and the shaft of the bolt. Examinations of failed bolts have made it possible to identify the cause of cracking as irradiation assisted stress corrosion cracking (IASCC). Up to now, baffle bolt cracking has been detected in units older than 15 years, where the baffle bolts are not cooled (no holes in the former to allow a water flow on the bolt shaft). In Belgium the concerned unit are Tihange 1 and Doel 1-2.The paper summarizes the experience with baffle bolts cracking in Belgian units and the strategy implemented to mitigate this problem, consisting of structural integrity analyses, baffle bolts inspections and replacement, and research programs in the field of IASCC, including examinations of highly irradiated replaced bolts.
机译:压板到隔板的螺栓用于压水反应堆中,以将隔板固定在反应堆容器下部内部的隔板上。所形成的结构形成了冷却剂流动的边界,并为燃料组件提供了横向支撑。也有一些边缘螺栓,将挡板组装在一起。 在大约120000小时的运行时间之后,一些螺栓在螺栓的头部和轴的接合处显示出裂纹。通过检查失效的螺栓,可以将裂纹的原因确定为辐射辅助应力腐蚀裂纹(IASCC)。到目前为止,在15年以上的装置中未检测到挡板螺栓开裂的情况,该装置未冷却挡板螺栓(前者中没有孔可让水流到螺栓轴上)。在比利时,有关部门是蒂昂格1号和杜尔1-2号。 这篇论文总结了比利时单位的挡板螺栓开裂的经验以及为减轻该问题而采取的策略,包括结构完整性分析,挡板螺栓的检查和更换以及IASCC领域的研究计划,包括对高辐射替换螺栓的检查。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号