ATOMIC SCALE INVESTIGATION OF NANOPARTICLE AND FABRICATION TEMPERATURE EFFECTS ON CARBON NANOTUBE DIAMETER AND CHIRALITY

机译:纳米颗粒的原子尺度研究和制造温度对碳纳米管直径和手性的影响

获取原文

摘要

Carbon nanotubes (CNTs) are one of the best candidates for utilizing in the future nanoelectronic devices. However, the semiconductivity property of CNTs varies as diameter and chirality number change. Several nanoelectronic applications require semiconductivity to be of a certain value with little variability. Therefore, it is necessary to reliably produce uniform CNTs with unique diameter and chirality. However, this still remains one of the challenging problems in the large scale production and application of CNTs. In this paper, the effect of fabrication temperature change on CNTs diameter and chirality are experimentally and theoretically studied. Utilizing chemical vapor deposition (CVD) fabrication process and by conducting experimental investigation, it is observed that a CNT possesses a larger diameter at its base compared to the section far away from deposited nanoparticles. Moreover, using MD simulation technique, it is observed that the energy of the CNTs molecular structure will increase by applying higher fabrication temperature. Usually this energy increase is greater in the thicker CNTs. However, the energy increase percentage is found to be affected by the chirality of the CNT. Among CNTs of the same diameter, the armchair conformation has the highest percent increase, followed by the chiral CNTs, and the zigzag nanotube has the lower percent increase. The obtained results can be utilized in a controllable CNTs diameter and chirality design process.
机译:碳纳米管(CNT)是在未来的纳米电子设备中使用的最佳候选材料之一。然而,CNT的半导电性质随着直径和手性数的变化而变化。几种纳米电子应用要求半导体具有一定的值且几乎没有变化。因此,必须可靠地生产具有独特直径和手性的均匀CNT。然而,这仍然是CNT的大规模生产和应用中的挑战性问题之一。本文通过实验和理论研究了制造温度变化对碳纳米管直径和手性的影响。利用化学气相沉积(CVD)的制造工艺,并通过实验研究,发现与远离沉积纳米颗粒的部分相比,CNT在其底部具有更大的直径。而且,使用MD模拟技术,观察到通过施加更高的制造温度,CNTs分子结构的能量将增加。通常,在较厚的CNT中,这种能量增加更大。然而,发现能量增加百分比受CNT的手性影响。在相同直径的CNT中,扶手椅构型的增加百分比最高,其次是手性CNT,而之字形纳米管的增加百分比较低。所得结果可用于可控制的CNT直径和手性设计过程中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号