Properties of Steam-Cured Fly Ash Concrete Using Porous Ceramic Waste Aggregate

机译:多孔陶瓷废骨料蒸养粉煤灰混凝土的性能

获取原文

摘要

In the present study, the effects of porous ceramic waste aggregate (PCWA) on the mechanical properties and durability of the steam-cured fly ash concrete are investigated. The replacement ratios of fly ash were 0%, 20% and 40% by mass, and those of PCWA were 0%, 10% and 20% by volume. Three kinds of curing conditions: dried after steam curing (D-Steam), sealed after steam curing (S-Steam), and sealed curing (Sealed), were used. The experimental results show that the compressive strength of the fly ash concrete with 20% replacement of PCWA increased regardless of curing conditions, and the pore volume decreased. The autogenous shrinkage of the S-Steam cured fly ash concrete was reduced significantly by using 20% replacement of PCWA. The carbonation resistance of the D-Steam cured fly ash concrete was also improved by using 10% replacement of PCWA and 40% replacement of fly ash.
机译:在本研究中,研究了多孔陶瓷废骨料(PCWA)对蒸汽养护的粉煤灰混凝土的机械性能和耐久性的影响。粉煤灰的置换率为0质量%,20质量%和40质量%,PCWA的置换率为0质量%,10质量%和20质量%。使用三种固化条件:蒸汽固化后干燥(D-Steam),蒸汽固化后密封(S-Steam)和密封固化(Sealed)。实验结果表明,在不考虑养护条件的情况下,添加20%PCWA的粉煤灰混凝土的抗压强度均得到提高,且孔体积减小。通过使用20%的PCWA替代量,S蒸汽固化的粉煤灰混凝土的自发收缩显着降低。通过使用10%的PCWA替代物和40%的粉煤灰替代物,D-Steam固化的粉煤灰混凝土的抗碳化性也得到了改善。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号