Effect of precursor concentration in the starting solution on the photocatalytic activity of ZnO thin films

机译:起始溶液中前驱体浓度对ZnO薄膜光催化活性的影响

获取原文

摘要

Undoped zinc oxide, ZnO, thin films were deposited on sodacalcic glass substrates by the ultrasonic spray pyrolysis technique, starting from zinc acetylacetonate as Zn precursor. Molar concentrations, varying in the 0.05-0.2M interval, were used. The ZnO thin films were deposited at different substrate temperatures, 375, 400, and 450°C. The photocatalytic characterization of ZnO thin films was performed by testing the degradation of an aqueous solution containing methylene blue (MB), at a concentration of 2.5×10 M, under UV irradiation, (15W Germicidal-UV lamp) for periods from 1 to 5 h. Absorbance of the solutions was measured by an UV-visible spectrophotometer at a wavelength of 664 nm. The variation of concentration of MB as a function of the irradiation time was calculated from the absorbance versus concentration calibrated curve. All films were characterized by XRD (X-ray diffraction), and ultraviolet-visible spectrophotometry. The XRD patterns confirmed the hexagonal wurtzite structure of the deposited ZnO films.
机译:通过超声喷雾热解技术,从乙酰丙酮锌作为锌前驱体开始,将未掺杂的氧化锌ZnO薄膜沉积在钠钙玻璃基板上。使用的摩尔浓度在0.05-0.2M区间内变化。 ZnO薄膜是在375、400和450°C的不同衬底温度下沉积的。 ZnO薄膜的光催化表征是通过测试含有亚甲基蓝(MB)的水溶液在2.5×10 M的紫外线辐射下(15W杀菌灯)在1至5的降解过程中进行的。 H。用紫外可见分光光度计在664nm的波长下测量溶液的吸光度。从吸光度对浓度校准曲线计算出MB浓度随照射时间的变化。所有膜均通过XRD(X射线衍射)和紫外可见分光光度法进行表征。 XRD图谱证实了沉积的ZnO薄膜的六方纤锌矿结构。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号