Characteristics degradation of gas transmission pipeline steel welded joints due to long-term operation

机译:长期使用会导致输气管道钢制焊接接头的特性降低

获取原文

摘要

The mechanical and electrochemical properties of different zones of welding joint of 17H1S pipe line steel after 30 years of service were investigated. It was established that long-term service causes a decrease of plasticity and impact toughness, especially of the heat affected zone metal. The weld metal revealed synchronous decrease of strength, hardness and brittle fracture resistance. Operated material revealed a general regularity of the potential shift to the negative direction for all zones of welded joint in comparison with those in the initial state. For the base metal, the potential shifts least, and, for the weld metal, it shifts most. So, selective corrosion can be localized on the weld metal with the increase of gas transmission pipelines service time.
机译:研究了使用了30年的17H1S管线钢焊接接头不同区域的力学和电化学性能。已经确定,长期使用会导致可塑性和冲击韧性,特别是热影响区金属的塑性和冲击韧性降低。焊缝金属显示出强度,硬度和脆性断裂强度同步下降。与初始状态下的材料相比,操作后的材料显示出焊接接头所有区域的电位向负方向移动的规律性。对于贱金属,电位偏移最小,而对于焊接金属,电位偏移最大。因此,随着气体传输管道使用寿命的增加,选择性腐蚀可局限在焊缝金属上。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号