The heavy metal in the waste can react with sulfur and be converted to metal sulfide through the hydrothermal sulfidation.For metal recovery,the synthetic metal sulfide can be enriched through subsequent flotation process.It is a novel way for the recovery of heavy metal from the sludge.In this study,the effects of liquid/solid ratio,mineralizer concentration,precursor concentration and dosage of sulfur on the sulfldation extent and floatation index were investigated.Result shows that with a precursor concentration of 15%,a Zn/S molar ratio of 1∶1.2,a liquid/solid ratio of 3∶1,the sulfidation extent of zinc in the sludge was greater than 92%,while the flotation recovery of zinc reached up to 45.34%.The toxicity characteristic leaching procedure (TCLP) revealed that stabilization and detoxification of heavy metals occurred during sulfidation.
机译:废物中的重金属可与硫反应,经水热硫化转化为金属硫化物。为回收金属,可通过后续的浮选工艺富集合成金属硫化物。这是一种从重金属中回收重金属的新方法。研究了液/固比,矿化剂浓度,前驱体浓度和硫的添加量对硫化程度和浮选指数的影响。结果表明,前驱体浓度为15%时,Zn / S摩尔比为比例为1∶1.2,液/固比为3∶1,污泥中锌的硫化程度大于92%,锌的浮选回收率高达45.34%。硫化过程中发生了重金属的稳定化和解毒作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号