Catalytic steam reforming of woody biomass was carried out with metal oxide supported Co catalysts. These catalysts were prepared by impregnation of Co2+ into SiO2, Y2O3 and CeO2 powder and sol-gel method for Co/MgO. Their catalytic activities were examined as hydrogen formation from steam reforming of woody biomass with as functions of reaction temperature. As the results, the highest amount of H2 formation shows Co/MgO at 973K while Co/SiO2 has maximum activity at 873K. This is because of activation of MgO basic site due to CO2 desorption from the active site. We suggest that the basicity of metal oxide supports affect the rate of steam reforming of tar rather than that of thermal decomposition of anhydrous cellulose.
机译:用金属氧化物负载的Co催化剂对木质生物质进行催化蒸汽重整。通过将Co 2 + 浸渍到SiO 2 ,Y 2 O 3 和CeO 中来制备这些催化剂Co / MgO的> 2 粉末和溶胶-凝胶法。考察了它们的催化活性,它是由木质生物质的水蒸气重整形成的氢形成的,并随反应温度的变化而变化。结果,最高量的H 2 形成在973K处显示Co / MgO,而Co / SiO 2 在873K处具有最大活性。这是由于CO 2 从活性位点解吸而激活了MgO碱性位点。我们建议金属氧化物载体的碱度影响焦油的蒸汽重整速率,而不是无水纤维素的热分解速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号