The potential of hot water extraction of birch wood chips followed by mild soda-anthraquinone pulping is investigated for the production of pure cellulosic pulp. Delignification in wood during a hot water extraction increases with temperature and extraction time, before condensation of lignin prevails. Furthermore, the removal of lignin appears to be governed by solubility, as indicated by the effect of the liquid-to-wood (L:W) ratio of the process. On the other hand, the L:W ratio has little effect on the removal of carbohydrates. A hot water treatment at 240 °C and a few minutes of extraction time, with a L:W ratio of 10:1 g/g, removes about 40% of the original lignin in wood. Under such operational conditions, all the hemicelluloses are extracted while the cellulose is hardly affected. The wood residue after the hot water extraction is further subjected to soda-anthraquinone pulping. The final pulp is composed of more than 95% pure cellulose, with a kappa number around 10. The final pulp yield, however, is less than 20% of the initial dry wood, owing to significant degradation of cellulose during the alkaline treatment.
机译:研究了热水提取桦木片的潜力,然后再进行温和的苏打蒽醌制浆,以生产纯纤维素纸浆。在木质素凝结之前,热水萃取过程中木材中的脱木素度随温度和萃取时间的增加而增加。此外,木质素的去除似乎受溶解度支配,如该方法的液木比(L:W)的影响所表明的。另一方面,L∶W比对碳水化合物的去除几乎没有影响。 L:W比为10:1 g / g的240°C热水处理和几分钟的萃取时间可去除木材中约40%的原始木质素。在这样的操作条件下,所有半纤维素都被提取,而纤维素几乎不受影响。热水萃取后的木材残留物进一步经过苏打-蒽醌制浆。最终的纸浆由超过95%的纯纤维素组成,kappa值约为10。但是,由于在碱性处理过程中纤维素的显着降解,最终的纸浆收率不到初始干燥木材的20%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号