In this paper, the effect of adding 1.0 wt.% Ce on the as-cast microstructure and mechanical properties of the Mg-3.8Zn-2.2Ca (wt.%) magnesium alloy were investigated. The results indicate that, after adding 1.0 wt.%Ce to the Mg-3.8Zn-2.2Ca alloy, small amounts of Mgi?Ce phase are formed and an obvious equiaxed trendance is observed. At the same time, the average grain size decreases from 234um to 71 um and the morphology of some Ca2Mg6Zn3 phases changes from initial coarse blocks to fine particles. In addition, adding 1.0 wt.%Ce to the Mg-3.8Zn-2.2Ca alloy also improve the tensile and creep properties of the alloy. Further investigations need to be considered in order to optimize the amounts of Ce additions and understand its effects on the tensile and creep properties and age-hardening behaviour.
机译:本文研究了添加1.0 wt。%Ce对Mg-3.8Zn-2.2Ca(wt。%)镁合金铸态组织和力学性能的影响。结果表明,向Mg-3.8Zn-2.2Ca合金中添加1.0 wt。%Ce后,形成少量的Mgi?Ce相,并观察到明显的等轴趋向。同时,平均晶粒尺寸从234um减小到71um,一些Ca2Mg6Zn3相的形态从最初的粗块变为细颗粒。另外,向Mg-3.8Zn-2.2Ca合金中添加1.0wt。%Ce也改善了合金的拉伸和蠕变性能。为了优化铈的添加量并了解其对拉伸和蠕变性能以及时效行为的影响,需要考虑进一步的研究。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号