ZrB2 powder has been prepared through carbothermal reduction boronization of zirconia/boron carbide/carbon mixtures heating assisted by microwave.The powder characteristics were investigated by X-ray diffraction (XRD),X-ray fluorescence (XRF),nitrogen absorption (BET model) and scanning electron microscope (SEM).The experiments indicated that excessive B4C is necessary and the carbothermic reaction reacts severely at a higher temperature and complete at 1600°C.The crystallite size has ranged from 50-100 nm,according to the calculated surface area.Highest purity of ZrB2 powder,which was synthesized at 1600°C,is 99.67 wt%.The surface area of ZrB2 powder synthesis at 1600°C is 18.33 m2/g.Vibration of temperature should affect the purity of ZrB2,as the sub reaction acted.
机译:通过微波辅助氧化锆/碳化碳/碳混合物加热的氧化锆/碳化物/碳混合物加热制备ZRB2粉末。通过X射线衍射(XRD),X射线荧光(XRF),氮吸收(BET模型)研究了粉末特性和扫描电子显微镜(SEM)。实验表明,需要过量的B4C,并且碳热反应在较高温度下严重反应,并在1600℃下完成。微晶尺寸范围为50-100nm,根据计算出的表面积。 。在1600℃合成的ZrB2粉末的高纯度为99.67wt%。1600℃的ZrB2粉末合成的表面积为18.33m 2 / g.振动应影响ZRB2的纯度,为亚反应作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号