In this study, a hydrometallurgical treatment involving solvent extraction of zinc using D2EHPA (di-2-ethylhexyl phosphoric acid) has been investigated to recover zinc from an industrial zinc leach residue. The residue was leached with sulfuric acid producing leach liquor which was subjected to solvent extraction for enrichment of zinc and removal of impurities. Operating variables for the zinc extraction process, such as pH of the mixed solution (0.5~5.0), concentration of D2EHPA (5%~40%,w/w), temperature (25~60°C), A/O volumetric phase ratio (1/2~4/1), concentration of tri-butyl phosphate (TBP) as modifier (3%~7%, w/w), concentration of Na2SO4 in aqueous phase (0.05M,0.1M, 0.2M) were also studied. Practically all zinc was extracted from the aqueous solution at pH 2.5 with 20% w/w D2EHPA in kerosene. At this operating condition, zinc could be extracted at one theoretical stage at A/O phase ratio of 1/1, as calculated by the McCabe-Thiele method.
机译:在该研究中,研究了涉及使用D2ehPA(二-2-乙基己基磷酸)的溶剂萃取锌的液压冶金处理,以从工业锌浸出残留物中回收锌。将残余物用硫酸生产浸出液浸出,溶剂萃取锌富集并除去杂质。用于锌提取过程的操作变量,如混合溶液的pH(0.5〜5.0),D2ehPa的浓度(5%〜40%,w / w),温度(25〜60℃),A / O容量相位比例(1/2〜4/1),磷酸三丁基(TBP)浓度为改性剂(3%〜7%,w / w),水相中Na 2 SO 4的浓度(0.05m,0.1m,0.2m)还研究了。实际上,所有锌都从pH 2.5的水溶液中用20%w / w d2ehpa溶液中萃取。在这种操作条件下,通过McCabe-Thiele方法计算,可以在1/1的一个理论阶段以一个理论阶段提取锌。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号