In this study, a hydrometallurgical treatment involving solvent extraction of zinc using D2EHPA (di-2-ethylhexyl phosphoric acid) has been investigated to recover zinc from an industrial zinc leach residue. The residue was leached with sulfuric acid producing leach liquor which was subjected to solvent extraction for enrichment of zinc and removal of impurities. Operating variables for the zinc extraction process, such as pH of the mixed solution (0.5~5.0), concentration of D2EHPA (5%~40%,w/w), temperature (25~60°C), A/O volumetric phase ratio (1/2~4/1), concentration of tri-butyl phosphate (TBP) as modifier (3%~7%, w/w), concentration of Na2SO4 in aqueous phase (0.05M,0.1M, 0.2M) were also studied. Practically all zinc was extracted from the aqueous solution at pH 2.5 with 20% w/w D2EHPA in kerosene. At this operating condition, zinc could be extracted at one theoretical stage at A/O phase ratio of 1/1, as calculated by the McCabe-Thiele method.
机译:在这项研究中,已进行了湿法冶金处理,其中涉及使用D2EHPA(二-2-乙基己基磷酸)对锌进行溶剂萃取,以从工业浸锌残渣中回收锌。用产生硫酸的浸出液浸出残余物,将其进行溶剂萃取以富集锌并去除杂质。锌萃取过程的操作变量,例如混合溶液的pH(0.5〜5.0),D2EHPA浓度(5%〜40%,w / w),温度(25〜60°C),A / O体积相比例(1/2〜4/1),磷酸三丁酯(TBP)作为改性剂的浓度(3%〜7%,w / w),水相中Na2SO4的浓度(0.05M,0.1M,0.2M)还进行了研究。实际上,所有的锌都是从pH 2.5的水溶液中以20%w / w的D2EHPA的煤油溶液提取的。在这种操作条件下,可以按照理论值,通过McCabe-Thiele方法计算,在A / O相比为1/1的情况下提取锌。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号