Weldability Evaluation and Nugget Formation Mechanism in Three Sheets Spot Welding of High Strength Steels

机译:高强度钢三张焊接焊接性评价与熔核形成机制

获取原文

摘要

The current trends of automotive industry are to reduce the weight of vehicle to increase fuel efficiency and also to improve the crash worthiness. These two properties hinder the improvement of each others. In the purposes of optimizing these two properties, three sheets spot welding of advanced high strength steel is introduced in automobile industry. The present study focused on the weldability of three sheets spot welding. Nugget growth mechanism and expulsion criteria were also evaluated. Weldability of (GA SGARC (0.7t) + Al-HPF (l.2t) + DP 590 (l.4t)) and (GA SGARC (0.7t) + TRIP 780 (l.2t) + DP 590 (1.4t)) was determined. Though based on button dia Al-HPF combination shows better weldable current range than TRIP combination but on the basis of weld strength both combinations having weldable current range of 1.5kA.The more reduction in weldable current range for Al-HPF combination compared to the TRIP combination attributed to the high button diameter for TRIP combinations. In earlier cycle of welding, heat generation for TRIP combination was occurring mostly in interface of thick-thick sheet and nugget growth rate was high in sheet direction. For Al-HPF combination significant amount of heat was generated in both interfaces due to the resistive Al-Si coating layer and nugget growth rate was high in electrode direction. Melting was observed at thick-thick sheet interface as well as geometric centre of middle sheet of Al-HPF combination. The expulsion was noticed in thick-thick sheet interface for both combinations. The higher temperature in thick-thick sheet interface for TRIP combination cause earlier expulsion in TRIP combination.
机译:汽车行业目前的趋势是减少车辆的重量,以提高燃油效率,也可以提高撞车效率。这两个物业阻碍了彼此的改善。以优化这两个性能的目的,在汽车工业中引入了先进的高强度钢的三张纸张点焊。本研究专注于三张焊接焊接的可焊性。还评估了金块增长机制和驱逐标准。 (GA SGA(0.7T)+ Al-HPF(L.2T)+ DP 590(L.4T))和(GA SGA(0.7T)+跳闸780(L.2T)+ DP 590(1.4T)的焊接性)确定。虽然基于按钮DIA - HPF组合显示比行程组合更好的可焊接电流范围,但基于焊接强度的焊接强度,两种可焊接电流范围为1.5ka的组合。与跳闸相比,Al-HPF组合的可焊接电流范围的可焊接电流范围的减少更大组合归因于跳闸组合的高按钮直径。在早期的焊接循环中,在厚厚的片材界面中发生跳闸组合的发热,并且块的钢疙瘩在纸张方向上高。对于Al-HPF组合,由于电阻Al-Si涂层,在两个接口中产生大量热量,并且电极方向块状生长速率高。在厚厚的薄板界面以及Al-HPF组合的几何中心观察到熔化。在厚厚的薄板界面中注意到这两种组合的驱逐。用于跳闸组合的厚厚厚的薄板界面中的较高温度导致跳闸组合的较早驱逐。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号