Effect of Epoxy Adhesive on Nugget Formation in Resistance Welding of SAE1004/DP600/DP780 Steel Sheets

机译:环氧胶粘剂对SAE1004 / DP600 / DP780钢板电阻焊接熔核形成的影响。

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

This study focused on the nugget formation in resistance welding of three dissimilar steel sheets influenced by different types and thicknesses of epoxy adhesive. An improved finite element model was employed to estimate the temperature distribution in three-sheet weld-bonding and was validated by the metallographic tests. Results showed that the weld initiation time and corresponding nugget size for weld-bonds would be earlier and larger than that of resistance spot welds in term of the same welding parameters. Compared to the adhesive Betamate Flex, the weld-bonding joint of three-sheets with adhesive Terokal 5089 would have a greater increment of the weld nugget sizes due to the increase of the static contact resistance brought by the interfaces between the steel sheets. However, the bond line thickness of the previously mentioned adhesive would take little effect on the weld sizes in weld-bonding of three dissimilar steel sheets.
机译:这项研究的重点是在三种不同钢板的电阻焊接中,熔核的形成受环氧胶类型和厚度的影响。采用改进的有限元模型来估计三层焊接中的温度分布,并通过金相测试进行了验证。结果表明,就相同的焊接参数而言,焊缝的焊接起始时间和相应的熔核大小将比电阻点焊的时间更早且更大。与粘合剂Betamate Flex相比,由于钢板之间的界面带来的静态接触电阻的增加,三层板与粘合剂Terokal 5089的焊接结合接头将具有更大的熔核尺寸增量。但是,在三种异种钢板的焊接中,上述粘合剂的结合线厚度对焊接尺寸几乎没有影响。