An analysis is developed which permits fatigue lifetimes of components with pre-existing crack-like defects to be represented by a single expression which is a function of stress range and initial defectsize; this is designated the Fatigue Intensity Factor (FIF). A greaphical representation indicates that all such failures will fall upon a single, flat surface. The conventional S-N curve is shown to be a special case of this surface. Outliers from this surface many inducate deficencies in testimates of stress range, of initial crack length, or that the failure is not due solely to fatigue. An equivalent analysis based upon the concent of threshold stress intensity indicates that a second, flat, intersecting surface exists. The conventional 'fatigue limit' often shown on S-N plots is shown to be a special case of this surface. Existing experimental data are used to define the surface, and examples of its application to the ordering of several potential fatigue locations within a single system and to interpreting non-standard fatigue failure are described.
机译:开发了一种分析方法,该方法允许将具有预先存在的裂纹状缺陷的组件的疲劳寿命用一个表达式表示,该表达式是应力范围和初始缺陷大小的函数;这被称为疲劳强度因子(FIF)。图形表示所有此类故障将落在单个平坦的表面上。常规的S-N曲线显示为该表面的特例。该表面的异常值在应力范围,初始裂纹长度的证明中引起许多缺陷,或者该失效并非仅是由于疲劳引起的。基于阈值应力强度的浓度的等效分析表明存在第二个平坦的相交表面。通常在S-N图上显示的常规“疲劳极限”是该表面的一种特殊情况。现有的实验数据用于定义表面,并描述了将其应用到单个系统中多个潜在疲劳位置的排序以及解释非标准疲劳破坏的示例。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号