The EFFECT OF STRAIN-HARDENING ON PWSCC OF NICKEL-BASE ALLOYS 600 AND 690

机译:应变硬化对镍基合金600和690的PWSCC的影响

获取原文

摘要

Stress corrosion cracking (SCC) behavior of base metals, cold-worked base metals and heat-affected zones (HAZs) in Alloy 600MA/Alloy 182 and Alloy 690TT/Alloy 52 welds in simulated PWR primary water environments is investigated. Hardness measurements and electron backscatter diffraction measurements show a hardened area in the heat-affected zones. Grain boundary chemistries and carbide precipitations were analyzed by Auger Electron Spectroscopy of the exposed intergranular fracture surface. Alloy 690TT base metal and Alloy 690TT HAZ show high SCC resistance. Extensive IGSCC was found in the Alloy 600MA HAZ, 8% and 20% cross-rolled (2DCR) Alloy 600MA materials, while mixed intergranular/transgranular SCC was found in the 40% CR Alloy 600MA specimens. The crack growth rate in the Alloy 600MA HAZ is close to that in the 8% 2DCR base metal, which is significantly lower than that in the 20% 2DCR base metal, but significantly higher than that in the as-received Alloy 600MA base metal.
机译:研究了在模拟PWR初级水环境中600MA / Alloy 182和690TT / Alloy 52合金焊缝中贱金属,冷加工贱金属和热影响区(HAZ)的应力腐蚀开裂(SCC)行为。硬度测量和电子背散射衍射测量显示了热影响区的硬化区域。通过暴露的晶间断裂表面的俄歇电子能谱分析了晶界化学和碳化物沉淀。 690TT合金贱金属和690TT HAZ合金具有较高的抗SCC性能。在600MA HAZ合金,8%和20%交叉轧制(2DCR)合金600MA材料中发现了广泛的IGSCC,而在40%CR合金600MA标本中发现了晶间/晶间混合SCC。合金600MA HAZ的裂纹扩展率接近8%2DCR基础金属的裂纹扩展率,该裂纹增长率明显低于20%2DCR基础金属的裂纹扩展率,但显着高于原定的合金600MA HAZ的裂纹扩展率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号