Noranda Inc., CEZinc presently employs a cement-stabilization (jarofix) process to stabilize its jarosite residues for direct disposal. In this process, Portland cement partly decomposes Na-jarosite to form Ca_6Fe_2(SO_4)_3(OH)_(12).nH_2O, ferric hydroxide and sodium sulphate which further reacts to form gypsum; approximately one-third of the Na-jarosite reacts in the current commercial product. The cured jarofix products also contain minor amounts of various Ca-Al-Fe silicate-sulphate-hydrate phases and traces of calcite. Together with gypsum and a Ca-Fe sulphate phase, these species bond the various particles together, imparting mechanical strength and reducing the permeability. Water-soluble Zn and Mg are stabilized in the Ca-Al-Fe silicate-sulphate-hydrate phases. The freshly cured products usually contain small amounts of moisture and traces of residual Portland cement, which provides additional alkalinity for the neutralization of any residual acid species. Jarofix products stored for more than six years in the laboratory, after curing, are usually dry and exhibit the same micro-textures as those of the freshly cured products. However, the stored products are depleted in the Ca_6Fe_2(SO_4)_3(OH)_(12).nH_2O and Portland cement phases, and are enriched in gypsum and calcite which reflects the highly alkaline environment of the jarofix products. The aged products also have increased amounts of the Ca-Al-Fe silicate-sulphate-hydrate phases which have elevated Zn and Mg contents. This implies a further immobilization of residual water-soluble Zn and Mg during storage.
机译:CEZinc的Noranda Inc.目前采用水泥稳定化(jarofix)工艺来稳定其黄钾铁矾残留物,以便直接处理。在此过程中,波特兰水泥将部分钠铁矿分解,形成Ca_6Fe_2(SO_4)_3(OH)_(12)。nH_2O,氢氧化铁和硫酸钠进一步反应形成石膏。在目前的商业产品中,约有三分之一的钠铁矾会发生反应。固化的jarofix产品还包含少量的各种Ca-Al-Fe硅酸盐-硫酸盐水合物相和痕量方解石。这些物质与石膏和Ca-Fe硫酸盐相结合,将各种颗粒粘合在一起,从而赋予机械强度并降低了渗透性。水溶性Zn和Mg在Ca-Al-Fe硅酸盐-硫酸盐-水合物相中稳定。新鲜固化的产品通常包含少量的水分和痕量的残留硅酸盐水泥,这为中和任何残留的酸物质提供了额外的碱度。固化后,Jarofix产品在实验室中存放超过6年通常是干燥的,并具有与新鲜固化产品相同的微观纹理。但是,所储存的产品耗尽了Ca_6Fe_2(SO_4)_3(OH)_(12).nH_2O和硅酸盐水泥相,并且富含石膏和方解石,这反映了jarofix产品的高度碱性环境。时效产品还具有增加的Zn-Mg含量的Ca-Al-Fe硅酸盐-硫酸盐-水合物相。这意味着在储存过程中残余水溶性锌和镁的进一步固定化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号