Boron carbide is one of the hardest materials known. The research on the synthesis of nano-sized boron carbide is of great importance. RF plasma synthesis of B_4C nano-particle was carried out by powder feeder using micro-sized commercial boron carbide powder as the stating material. Different plasma energy and powder feeder probe position was used to find out the optimum condition to achieve nanoparticles. Powders were collected from Chamber 1, 2 and 3. fine particles can be achieved, but the decomposition and oxidation of B_4C powder during the high temperature plasma spray was detected. Boron oxide was found in the sprayed powder, and the powder was purified by washing and heat treatment. XRD, SEM and TEM was used to for characterization of the particles.
机译:碳化硼是已知的最硬的材料之一。纳米碳化硼的合成研究具有重要意义。 B_4C纳米粒子的RF等离子体合成是通过粉末进料器进行的,使用的是微型碳化硼粉末作为原料。使用不同的等离子体能量和粉末进料器探针位置来找出获得纳米颗粒的最佳条件。从第1、2和3室收集了粉末,但可以看到B_4C粉末在高温等离子喷涂过程中的分解和氧化。在喷雾粉末中发现氧化硼,并通过洗涤和热处理将粉末纯化。 XRD,SEM和TEM用于表征颗粒。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号