In order to develop the high efficiency and regenerable zinc-based sorbent for hot gas desulfurization, zinc-based sorbnets with ZrO_2 as an additive was studied. Zinc-based sorbents were prepared by the solid mixing method. The sulfidation and regeneration tests for H_2S removal efficiency of zinc-based sorbents were carried out in the fixed-bed tubular reactor system. The sulfidation and regeneration temperatures were 480℃ and 580℃, respectively. The concentration of H_2S in coal gas was about 10000 ppmv. The sulfidation and regeneration rate of zinc-based sorbents were measured by Cahn-balance(D-200). The physical-chemical properties of zinc-based sorbents were characterized by SEM etc. From the results, it was found that ZrO_2 improved the regenerability and the durability of zinc-based sorbents during multi-cyclic tests. Specially, the regeneration rate of zince-based sorbent with ZrO_2 was higher at high temperature than that of the other sorbents.
机译:为了开发用于热气脱硫的高效可再生锌基吸附剂,研究了以ZrO_2为添加剂的锌基吸附剂。锌基吸附剂通过固相混合法制备。在固定床管式反应器系统中对锌基吸附剂的H_2S去除效率进行了硫化和再生测试。硫化温度为480℃,再生温度为580℃。煤气中H_2S的浓度约为10000 ppmv。用Cahn-balance(D-200)测定锌基吸附剂的硫化和再生速率。通过SEM等对锌基吸附剂的物理化学性质进行了表征。结果表明,ZrO_2在多循环试验中提高了锌基吸附剂的可再生性和耐久性。特别地,在高温下,ZrO_2对锌基吸附剂的再生速率高于其他吸附剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号