The microstructural study of a direct laser deposited Ti alloy

机译:直接激光沉积钛合金的显微组织研究

获取原文
获取原文并翻译 | 示例

摘要

The alloy Ti25V15Cr2A10.2C(wt%) has been developed as a burn-resistant Ti alloy and as such it has potential for blade tipping. The technique of laser deposition has been used to build up solid material from the powdered alloy on Ti6A14V substrates. The present work is concerned mainly with assessing the microstructure of laser-deposited samples of this alloy after deposition. The mechanical properties of this alloy are controlled by the presence of TiC precipitates, which control grain growth during conventional thermo-mechanical processing and which also getter the matrix alloy of oxygen. Hence one of the microstructural features which has been assessed in some detail is the distribution of the TiC precipitates formed after laser deposition.
机译:Ti25V15Cr2A10.2C(wt%)合金已被开发为一种耐燃的Ti合金,因此它有可能导致叶片倾翻。激光沉积技术已被用来在Ti6A14V基板上由粉末状合金堆积固体材料。本工作主要涉及评估沉积后该合金的激光沉积样品的显微组织。该合金的机械性能由TiC沉淀物的存在控制,该沉淀物在常规热机械加工过程中控制晶粒的生长,并且还会吸收氧气的基体合金。因此,已被详细评估的微观结构特征之一是在激光沉积后形成的TiC沉淀物的分布。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号