PREPARATIONTECHNIQUE AND PERFORMANCE STUDY OF CONSTRUCTION WASTE RECYCLED COARSE AND FINE AGGREGATE CONCRETE

机译:废旧粗骨料和细骨料混凝土的制备技术及性能研究

获取原文
获取原文并翻译 | 示例

摘要

This paper studies the preparation technology of recycled coarse and fine aggregate concrete, and on the basis of the dense packing of aggregate, implements the studies in the effects on the performance of concrete through the adjustment for the different contents of recycled fine aggregate and fly ash, as well as for different water-binder ratios, so as to determine the design principle and technical route to the mixing ratio of recycled concrete. It is suggested that the blended ratio of recycled fine aggregate in the fine aggregates should be appropriately controlled within 50%;the blended ratio of fly ash in the cementing materials should be appropriately controlled within 30-35%;with the increase of fly ash content, the each-age strength of concrete should be ensured through the decrease of water-binder ratio under the premise that the volume of pasty remains unchanged, and the water-binder ratio should not exceed 0.40. In addition, testing result indicates that prewet recycled fine aggregate is an effective technical measure to control slump loss and has no great impact on the strength.
机译:本文研究了再生粗,细骨料混凝土的制备技术,在骨料密实填充的基础上,通过调整再生细骨料和粉煤灰的不同含量,对混凝土的性能进行了研究。 ,以及不同的水粘结剂比例,从而确定再生混凝土的配合比的设计原理和技术路线。建议将再生细骨料在细骨料中的混合比例控制在50%以内;胶凝材料中粉煤灰的混合比例应控制在30-35%以内;随粉煤灰含量的增加,应在胶泥体积不变的前提下,通过降低水灰比来保证混凝土的每龄强度,水灰比应不超过0.40。另外,测试结果表明,预湿再生细骨料是控制坍落度损失的有效技术手段,对强度没有太大影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号