It is known that bolt forces reduce significantly after tightening bolted flanged connections in which expanded PTFE gaskets are used. Bolts are often post-tightened in practice after initial tightening to compensate for the reduction of bolt forces. The viscoelastic characteristic of expanded PTFE gaskets is thought to be the main cause for the phenomenon. Some gasket users are not confident whether the bolt forces remain above a minimum required gasket load until next maintenance. However, the long term characteristics of the residual bolt forces and the sealing performance of flanged connections have not been clarified yet. In this study, using flanged connections with expanded PTFE gaskets, the reduction of bolt forces and the change in the sealing performance were measured at room temperature for one year. Based on the test results, the residual bolt force and the sealing performance were studied. It was clarified that bolt forces converges to a certain level at early stage within almost 1000 hours. After that, the bolt forces were significantly affected by the ambient temperature change. This is because the thermal expansion of PTFE material is high and also the thermal characteristic of PTFE material has a temperature dependency. It was confirmed that although the bolt force reduced significantly at early stage, it is maintained in long-term. The sealing performance was improved due to the increased compression of gasket.
机译:众所周知,在拧紧使用膨胀PTFE垫圈的螺栓法兰连接后,螺栓力会大大降低。在实践中,螺栓通常在初始拧紧后进行后拧紧,以补偿螺栓力的减小。膨胀的PTFE垫圈的粘弹性特性被认为是造成这种现象的主要原因。一些垫圈用户不确定螺栓力是否保持在最小所需垫圈载荷以上,直到下次维护。但是,残余螺栓力的长期特性和法兰连接的密封性能尚未弄清。在这项研究中,使用法兰连接和膨胀的PTFE垫圈,在室温下测量了一年内螺栓力的减小和密封性能的变化。根据测试结果,研究了残余螺栓力和密封性能。明确了螺栓力在近1000小时内在早期收敛到一定水平。之后,螺栓力受环境温度变化的影响很大。这是因为PTFE材料的热膨胀高,并且PTFE材料的热特性也具有温度依赖性。可以肯定的是,尽管螺栓力在早期阶段显着降低,但可以长期保持。由于增加了垫圈的压缩,因此改善了密封性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号