ANSLC ARTIFICIAL NEURAL STRAIN LIFE CURVES

机译:ANSLC人工神经应变寿命曲线

获取原文
获取原文并翻译 | 示例

摘要

A durable design for linear flow split sheet components requires suitable methods and transferability criteria which are not yet available for dentritic structures. Knowledge of the cyclic material behaviour is essential for this. For this reason, the cyclic material parameters are determined as a function of the product's properties (level of deformation, microstructure, surface finish, residual stresses) and different loading parameters. However, since the determination of the cyclic parameters is associated with considerable experimental effort and costs, a cost-effective and easy method is sought to determine these parameters. A very promising approach for this is the application of artificial neural networks (ANN) since they have the ability to generate the influences on the fatigue strength from the manufacturing and environmental parameters using sensibly selected input parameters. They offer the possibility to access acquired knowledge and to thus construct a multidimensional map based on a few tests.
机译:线性分流片部件的耐用设计需要合适的方法和可转移性标准,而这些方法和可塑性标准尚不适用于树状结构。为此,了解循环材料的行为至关重要。因此,应根据产品性能(变形水平,微观结构,表面光洁度,残余应力)和不同的加载参数确定循环材料参数。然而,由于循环参数的确定与相当大的实验努力和成本相关联,因此寻求一种成本有效且容易的方法来确定这些参数。一种非常有前途的方法是应用人工神经网络(ANN),因为它们能够使用合理选择的输入参数从制造和环境参数中产生对疲劳强度的影响。他们提供了访问获得的知识并因此基于一些测试构建多维图的可能性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号