The present paper investigates specific sustained crushing stress (SSCS) of various composite laminate designs and stiffened boxes under axial crushing test. In this regard, an optimum composite crash box design is sought by studying the effect of laminate design and stiffeners on SSCS. Crash boxes were fabricated from carbon/epoxy twill-weave fabrics of [0]_4, [45]_4 and [0,45]_2. The progressive failure with three distinct crushing modes of transverse shearing, lamina bending and brittle fracture was observed for three laminate designs. Two new assembled composite boxes were made from channels and V-shape stiffener and tested in quasi-static condition. Adhesive bonding was used in joining the channelled and stiffened boxes. Measured amount of SSCS for all models were compared to find an optimum crash box. It was found SSCS increases with increasing proportion of 0° plies in the laminate.
机译:本文研究了各种复合材料层压板设计和加劲箱在轴向压碎试验下的比持续压碎应力(SSCS)。在这方面,通过研究层压板设计和加劲肋对SSCS的影响,寻求一种最佳的复合防撞箱设计。碰撞盒由碳纤维/环氧斜纹编织织物[0] _4,[45] _4和[0,45] _2制成。对于三种层压板设计,观察到具有三种不同的横向剪切,层板弯曲和脆性断裂破碎模式的渐进破坏。两个新组装的复合材料盒由通道和V形加劲肋制成,并在准静态条件下进行了测试。粘合剂用于连接槽形和刚性的盒子。比较所有模型的SSCS量,以找到最佳的碰撞盒。发现SSCS随着层压物中0°层的比例增加而增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号