Ti6Al4V is widely used in the aerospace industry due to its lightweight and high strength properties. Joining titanium is of prime importance and while other welding techniques have been documented, the use of a fibre laser to weld this material has not been extensively investigated. In this paper, autogenously butt weld joints of thin sheet of Ti6Al4V were carried out using a 2 kW Ytterbium fibre laser. To investigate the suitable welding experiment condition the welds were performed at different shielding conditions then the effects of laser power, welding speed, shielding gas on the fusion zone width of Ti6Al4V have been analyzed. The results suggest that in order to achieve a full penetration, minimum fusion zone and acceptable weld profile with low distortion for thin sheet titanium, the combination of process parameters should be carefully considered.
机译:Ti6Al4V的重量轻且强度高,因此广泛用于航空航天工业。连接钛至关重要,尽管已记录了其他焊接技术,但尚未广泛研究使用光纤激光器焊接这种材料。在本文中,使用2 kW fiber光纤激光器对Ti6Al4V薄板进行自对接焊接。为了研究合适的焊接实验条件,在不同的保护条件下进行焊接,然后分析了激光功率,焊接速度,保护气体对Ti6Al4V熔合区宽度的影响。结果表明,为了实现薄钛板的完全熔深,最小熔合区和可接受的焊接轮廓且变形低,应仔细考虑工艺参数的组合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号