A commercial Oxidation Induction Time (OIT) reference material polyethylene film is retested six years after its original certification. Using ASTM International Standard E1SS8, the mean value, within laboratory repeatability and between laboratory reproducibility are unchanged at 29.3 min, 1.7 and 2.1 min, respectively. In addition the new results are reported on an interlaboratory test for Oxidation Onset Temperature (OOT) for the same material using Method A (oxygen purge gas) and C (air purge gas) of ASTM Standard E2009. The mean values are found to be 236.8 and 245.0℃ under oxygen and air, respectively. The within laboratory repeatability standard deviation is 1.1 and 0.68℃, and the between laboratory reproducibility standard deviation is 1.3 and 1.4℃, respectively for oxygen and air.
机译:商业氧化诱导时间(OIT)参考材料聚乙烯薄膜在其原始认证后的六年内进行了重新测试。使用ASTM国际标准E1SS8,实验室可重复性内和实验室可重复性之间的平均值分别保持在29.3分钟,1.7分钟和2.1分钟不变。此外,在ASTM Standard E2009的方法A(氧气吹扫气体)和C(空气吹扫气体)对同一材料进行氧化起始温度(OOT)的实验室间测试中,报告了新结果。在氧气和空气下,平均值分别为236.8和245.0℃。氧气和空气的实验室可重复性标准偏差为1.1和0.68℃,实验室可重复性标准偏差为1.3和1.4℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号