Upconversion luminescence of KGd(MoO4)2: Er3+,Yb3+ powder prepared by the Pechini method

机译:Pechini法制备的KGd(MoO4)2:Er3 +,Yb3 +粉末的上转换发光

获取原文
获取原文并翻译 | 示例

摘要

Er3+doped potassium gadolinium molybdate (KGM) phosphor with sensitizer Yb3+ion has been synthesized by the Pechini method using citric acid and enthyleneglycol. The crystallization processes of the phosphor precursors were characterized by X-ray diffraction (XRD) and thermogravimetry-differential scanning calorimetry (TG-DSC), which indicated that ultrafine uniform crystallites of KGM:Er,Yb were obtained by sintering the precursors at above 650℃ for 5h. Upconversion luminescence (UL) spectra of the samples were studied by a 976 nm semiconductor laser diode (LD) excitation. The UL spectra exhibited the green and red emission bands that were attributed to the 2H11/2, 4S3/2→4I15/2 and 4F9/2→4I15/2 transitions of Er3+, respectively. The occurence of UL can be attributed to a two-photon process. The maximum luminescent intensity was achieved when the concentration of Er3+, Yb3+arrived at 1 mol% and 20 mol%, respectively.
机译:用柠檬酸和乙二醇通过Pechini方法合成了具有增感剂Yb3 +离子的Er3 +掺杂的钼酸钾g(KGM)荧光粉。通过X射线衍射(XRD)和热重分析-差示扫描量热法(TG-DSC)表征了磷光体前驱体的结晶过程,表明在650℃以上的温度烧结得到了KGM:Er,Yb超细均匀的晶体。 ℃5h。通过976 nm半导体激光二极管(LD)激发研究了样品的上转换发光(UL)光谱。 UL光谱显示绿色和红色发射带,分别归因于Er3 +的2H11 / 2、4S3 / 2→4I15 / 2和4F9 / 2→4I15 / 2跃迁。 UL的出现可归因于双光子过程。当Er3 +,Yb3 +的浓度分别达到1mol%和20mol%时,获得最大发光强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号