The mechanical properties of reinforced plastic mortar (RPM) pipe material are typically measured prior to production in order to establish design properties, and during production to ensure quality of the pipe material. Seldom does the opportunity become available to measure the mechanical properties of service-aged (conditioned) components. In this paper, the short-term properties of the service-aged pipes are compared with the original production specifications. The long-term, strain-corrosion cracking properties have also been measured during the past 10 years on these service-aged pipes. Some laboratory specimens still have not failed after 10 years under test. Reinforced plastic mortar (RPM) pipes were excavated from the ground after about 15 years of sewer service, and material coupons from these pipes were subjected to various mechanical tests. Axial-direction tensile tests, hoop-direction stiffness, and acid strain-corrosion testing were performed. The acid strain corrosion tests were monitored as a function of time until failure. The resulting lifetimes were related to the initial surface strains and showed a decreasing logarithmic relationship for both concentrations of the sulfuric acid solutions. Some pipe samples have been under test for 10 years, and prior to this testing were buried in the ground, and used as sewer pipes for 15 years. The failed laboratory specimens were compared by fractographic examination with those from in-service failures. Laboratory specimens that failed in shorter times appeared to be overload in nature and exhibited little, if any, time-dependent fracture surface features. In-service failures indicate that the crack had been present for a significant time. Comparisons are also made between the observed fractographic appearance of the fibers and the laboratory failure time for both pH values.
机译:为了确定设计性能,通常在生产之前测量增强塑料砂浆(RPM)管材料的机械性能,并在生产过程中确保其质量。很少有机会来测量已使用年限(调节)的组件的机械性能。在本文中,将使用寿命已久的管道的短期性能与原始生产规格进行了比较。在过去的十年中,还对这些使用年限的管道进行了长期的应变腐蚀开裂性能测试。经过10年的测试,一些实验室标本仍然没有失败。下水道服务大约15年后,从地下挖出了增强的塑料砂浆(RPM)管,并对这些管的材料挂片进行了各种机械测试。进行了轴向拉伸试验,环向刚度和酸应变腐蚀试验。监测酸应变腐蚀试验作为失效前时间的函数。最终的寿命与初始表面应变有关,并且两种浓度的硫酸溶液的对数关系均减小。一些管道样品已经进行了10年的测试,并且在测试之前被埋在地下,并用作下水道15年。通过分形检查将失效的实验室样本与在役失效的样本进行比较。在较短时间内失效的实验室标本在性质上似乎是超负荷的,并且几乎没有时间依赖性的断裂表面特征。在役故障表明裂缝已经存在了很长时间。还对观察到的纤维的分形外观和两个pH值的实验室破坏时间进行了比较。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号