Calcium Level-Responsive Zinc Ion Release from Tricalcium Phosphate Containing Zinc (ZnTCP)

机译:从含锌的磷酸三钙(ZnTCP)释放钙水平响应性锌离子

获取原文
获取原文并翻译 | 示例

摘要

Tricalcium phosphate containing Zn (ZnTCP; 0.63, 6.17 and 12.05 Zn w/wpercent) were investigated Zn~(2+) release from ZnTCP. The in-vitro release rates from Zn-TCP powders were measured in 25 ml of SBF containing 10 mg/100mL Ca~(2+)(SBF (H)), SBF containing 5 mg/100mL Ca~(2+) (SBF(L)) or SBF without Ca~(2+) (SBF(-)) at pH7.25, 37.0+0.1 deg C. The Zn~(2+) release rate from 6 and 12percent ZnTCP were much faster than that at the latter stage. The Zn~(2+) release rate from ZnTCP decreased with increasing Ca~(2+) concentration in dissolution media. The rate from ZnTCP increased with increasing Zn~(2+) concentration in TCP. On the other hand, the aqueous ZnTCP suspension containing 10mg of 6 and 12percent ZnTCP was subcutaneously injected into the backs of the ovarictomized female Wistar rats. The plasma Zn~(2+) levels at 1-5 days of ZnTCP loaded rats increased comparing with the control disease model. The area under the curve of Zn release profiles (AUC) of 6 and 12percentZnTCP were significantly higher than that of control disease model.
机译:研究了含Zn的磷酸三钙(ZnTCP; 0.63、6.17和12.05 Zn w / w%),研究了ZnTCP中Zn〜(2+)的释放。在25 ml含10 mg / 100mL Ca〜(2 +)(SBF(H))的SBF,5 mg / 100mL Ca〜(2+)(SBF)的SBF中测量Zn-TCP粉末的体外释放速率(L))或不含Ca〜(2+)的SBF(SBF(-))在pH7.25、37.0 + 0.1摄氏度下进行。ZnTCP(6%+ 12%)的Zn〜(2+)释放速率比在7%时的快得多后期。 ZnTCP中Zn〜(2+)的释放速率随溶解介质中Ca〜(2+)浓度的增加而降低。 ZnTCP的速率随TCP中Zn〜(2+)浓度的增加而增加。另一方面,将含有10mg 6和12%ZnTCP的ZnTCP水溶液悬浮液皮下注射到卵巢切除的雌性Wistar大鼠的背部。与对照疾病模型相比,ZnTCP负荷的大鼠在1-5天时血浆Zn〜(2+)水平升高。锌释放曲线(AUC)的曲线下面积分别为6%和12%ZnTCP,显着高于对照疾病模型。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号