首页> 外国专利> METHOD FOR APPLICATION OF ELECTROEROSION-RESISTANT COATINGS BASED ON SILVER, COBALT AND COBALT NITRIDES ON COPPER ELECTRICAL CONTACTS

METHOD FOR APPLICATION OF ELECTROEROSION-RESISTANT COATINGS BASED ON SILVER, COBALT AND COBALT NITRIDES ON COPPER ELECTRICAL CONTACTS

机译:铜电触点上基于银、钴和氮化钴的抗电腐蚀涂层的应用方法

摘要

FIELD: electrical erosion-resistant coatings.;SUBSTANCE: invention relates to the formation of electrical erosion-resistant coatings on copper electrical contacts and can be used in electrical engineering. The method includes an electric explosion of a two-layer composite electrically exploded conductor, one of the layers of which consists of silver foil weighing 60-360 mg, and the second layer is made of cobalt foil equal to 0.5-2.0 mass of the first layer, the formation of pulsed multiphase plasma jet, its melting of the surface of a copper electrical contact at an absorbed power density of 4.5-6.5 GW/m2, deposition of explosion products on the surface and formation of a coating of the Co-Ag system on it, nitriding for 3-5 hours at a temperature of 500-600°C and subsequent pulse-periodic electron-beam treatment of the coating surface at an absorbed energy density of 40-60 J/cm2 , pulse duration 150-200 mcs and the number of pulses 10-30.;EFFECT: invention is aimed at obtaining electrical erosion-resistant coatings with high electrical conductivity, electrical erosion resistance and adhesion to the substrate at the level of cohesion.;1 cl, 3 dwg, 2 ex
机译:领域:抗电腐蚀涂层。;物质:本发明涉及在铜电触点上形成抗电腐蚀涂层,可用于电气工程。该方法包括两层复合电爆炸导体的电爆炸,其中一层由重量为60-360 mg的银箔组成,第二层由等于第一层质量0.5-2.0的钴箔制成,形成脉冲多相等离子体射流,以4.5-6.5 GW/m2的吸收功率密度熔化铜电触点表面,在表面沉积爆炸产物并在其上形成Co-Ag系统涂层,在500-600°C的温度下氮化3-5小时,然后以40-60 J/cm2的吸收能量密度对涂层表面进行脉冲周期性电子束处理,脉冲持续时间150-200 mcs,脉冲数10-30。;效果:本发明的目的是获得具有高导电性、抗电腐蚀性和在粘合水平上粘附于基材的抗电腐蚀涂层。;1个cl,3个图纸,2个ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号