The present disclosure relates to a medical silicon rubber having high mechanical property and a preparation method thereof. The medical silicon rubber comprises the following raw materials in parts by weight: 50˜90 parts of silicon rubber, 10˜50 parts of polyurethane, 10˜50 parts of fillers, 2˜6 parts of hydrogen-containing silicon oil and 2˜5 parts of a vulcanizing agent. The preparation method comprises: evenly mixing a part of fillers with silicon rubber in an internal mixer for later use, and evenly mixing the other part of fillers with polyurethane in the internal mixer; and mixing the mixed polyurethane on an open type rubber refining machine, then successively adding hydrogen-containing silicon oil, the evenly mixed silicon rubber and the vulcanizing agent into the open type rubber refining machine many times by small portions, and finally vulcanizing the mixed rubber on a plate rubber vulcanizing machine for 5˜15 min at 150˜190° C.
机译:本公开涉及一种具有高机械性能的医用硅橡胶及其制备方法。 医用硅橡胶包括以下重量份的原材料:50~90份硅橡胶,10〜50份聚氨酯,10〜50份填料,2〜6份含氢含氢硅油和2~5份。 硫化剂的一部分。 制备方法包括:在内部混合器中均匀地将含有硅橡胶的填料的一部分与内部混合器均匀地混合在内部混合器中用聚氨酯混合填料的另一部分; 并将混合聚氨酯混合在开放式橡胶精制机上,然后通过小部分依次将含氢含氢硅油,均匀混合的硅橡胶和硫化剂加入开放式橡胶精炼机中,最后硫化混合橡胶 在150~190℃下,在板材橡胶硫化机上5-15分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号