The cryogenic austenitic high-manganese steel having excellent corrosion resistance, according to one aspect of the present invention, comprises 0.2-0.5 wt % of C, 23-28 wt % of Mn, 0.05-0.5 wt % of Si, 0.03 wt % or less of P, 0.005 wt % or less of S, 0.5 wt % or less of Al, and 3-4 wt % of Cr, with the remainder being Fe and other unavoidable impurities, also comprises at least 95 area % of austenite as a microstructure, and has Cr concentration sections continuously formed within an area of 50 μm in the thickness direction from the surface, wherein the;Cr concentration sections comprise a high Cr concentration section having a relatively high concentration of Cr, and a low Cr concentration section having a relatively low concentration of Cr, and the high Cr concentration section maybe distributed at 30 area % or less (but not 0%) relative to the whole surface area of the Cr sections.
机译:根据本发明的一个方面,具有优异的耐腐蚀性的低温奥氏体高锰钢,包括0.2-0.5wt%的C,23-28wt%的Mn,0.05-0.5wt%的Si,0.03wt%或 较少的P,0.5wt%或更少的Al,0.5wt%或更少的Al,3-4wt%的Cr,其余部分是Fe和其他不可避免的杂质,还包含至少95个面积的奥氏体作为a 微观结构,并且Cr浓度部分在从表面的厚度方向上连续形成在50μm的面积内,其中Cr浓度部分包含具有相对高浓度Cr的高Cr浓度部分,并且具有低Cr浓度部分 相对于CR部分的整个表面积,相对较低的Cr浓度的Cr和高Cr浓度部分可以分布在30个面积%或更少(但不是0%)。

著录项

  • 公开/公告号US2021388475A1

    专利类型

  • 公开/公告日2021-12-16

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号US201917283884

  • 申请日2019-10-25

  • 分类号C22C38/38;C22C38/06;C22C38/20;C22C38/32;C22C38/02;C21D8/02;

  • 国家 US

  • 入库时间 2024-06-14 22:32:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号